For the Springer tungsten project near Imlay, Nevada, a mill-design question comes down to how much rock the plant would have to grind to reach the tungsten in it. On Monday, Blue Moon Metals reported that X-ray sorting separated a medium-grade stockpile sample into fractions. The selected fractions carried 93.3% of the sample’s tungsten oxide in 37.7% of its weight.
Put another way, for every 100 pounds of that test feed, about 38 pounds would go on to milling at that cut, leaving about 62 pounds out of the mill feed. About 7% of the sample’s tungsten oxide would be left behind at that stage. The calculation uses Table 4 of Blue Moon’s SEC exhibit. The share retained measures what ended up in the selected rock, before any losses from milling or later processing.
The low-grade test raises a separate question. Both the company’s website and the SEC exhibit put the selected material at 28.3% of the test feed by weight. The website puts its share of the sample’s tungsten oxide at 89.2%, while the exhibit gives 93.3%. The first two fractions in the exhibit’s Table 5 add up to 89.1% using the displayed rounded figures. The two versions leave the precise low-grade recovery unresolved.
Blue Moon says the Saskatchewan Research Council tested three samples assembled from older stockpiles. The lab’s description of its methods distinguishes initial tests of how rock responds to sensors from pilot testing on material as it comes out of a mine. For Springer, Blue Moon says it will review whether a sorter fits its proposed processing layout and look at assay results from other stockpiles as they become available. Monday’s results give the company a basis for that design work. The figures measure selected lab samples, so they leave open how much rock the mill would handle in operation.
Cover photo by James St. John / Wikimedia Commons, CC BY 2.0. Resized and cropped for display.